Tipo | Composición química | |||||||||
AWSA5.1 | AWS A5.1M | do | Minnesota | Si | PAG | S | NI | CR | Mes | V |
E6011 E6013 | E4311 E4313 | ≤0.20 | ≤1.20 | ≤1.00 | ... | ... | ≤0.30 | ≤0.20 | ≤0.30 | ≤0.08 |
E7016 E7018 | E4916 E4918 | ≤0.15 | ≤1.60 | ≤0.75 | ≤0.035 | ≤0.035 | ≤0.30 | ≤0.20 | ≤0.30 | ≤0.08 |
E7018M | E4918M | ≤0.12 | 0.40 ~ 1.60 | ≤0.80 | ≤0.030 | ≤0.020 | ≤0.25 | ≤0.15 | ≤0.35 | ≤0.05 |
E308-16 E308L-16 | E308-17 E308L-17 | ≤0.08 | 0.50 ~ 2.50 | ≤1.00 | ≤0.04 | ≤0.03 | 9.0 ~ 11.0 | 18.0 ~ 21.0 | ≤0.75 | Cu ≤0.75 |
≤0.04 | ||||||||||
E309 -16 E309L -16 | E309-17 E316-17 | ≤0.15 | 0.50 ~ 2.50 | ≤1.00 | ≤0.04 | ≤0.03 | 12.0 ~ 14.0 | 22.0 ~ 25.0 | ≤0.75 | Cu ≤0.75 |
≤0.04 | ||||||||||
E316-16 E316-16 | E316L-17 E309L-17 | ≤0.08 | 0.50 ~ 2.50 | ≤1.00 | ≤0.04 | ≤0.03 | 11.0 ~ 14.0 | 17.0 ~ 20.0 | 2.0 ~ 3.0 | Cu ≤0.75 |
≤0.04 | ||||||||||
E312-16 | E312-17 | ≤0.15 | 0.50 ~ 2.50 | ≤1.00 | ≤0.04 | ≤0.03 | 8.0 ~ 10.5 | 28.0 ~ 32.0 | ≤0.75 | Cu ≤0.75 |
Nota: Componentes E7016 y E7018 de Mn+Ni+Cr+Mo+VS1.75; Interpretación del código de electrodo de acero inoxidable-Ejemplo E308-XX (E308-15/E308-16/E308-17/E308-26 ... ...), el código de prefijos se dividió en -1/-2/4, representa la posición de soldadura; El código de sufijo se divide en -5L-6/-7, en el que 5 representa la alcalinidad, 6 representa rutilo y 7 representa el tipo de ácido titánico. |
Tipo | Propiedades mecánicas | ||||||
AWSA5.1 | AWS A5.1M | MPA de resistencia a la tracción | MPA de resistencia de rendimiento | Alargamiento a (%) | Valor de impacto | Radio gráficos | |
KV2 (J) -45 ℃ | Kv2 () -30 ℃ | ||||||
E6011 | E4311 | ≥430 | ≥330 | ≥22 | ... | ≥ 27 | Grado LL |
E6013 | E4313 | ≥430 | ≥330 | ≥17 | ... | ... | |
E7016 | E4916 | ≥490 | ≥400 | ≥22 | ≥ 27 | ≥ 27 | Grado L |
E7018 | E4918 | ≥490 | ≥400 | ≥22 | ≥ 27 | ≥ 27 | |
E7018M | E4918M | Normal ≥ 490 | 370 ~ 500 | ≥24 | ... | ≥ 67 | |
2.4 mm/370 ~ 530 | |||||||
E308-XX | ≥550 | ≥30 | |||||
E308L-XX | ≥520 | ||||||
E309-XX | ≥550 | ||||||
E309L-XX | ≥520 | ||||||
E316-XX | ≥520 | ||||||
E316L-XX | ≥490 | ||||||
E312-XX | ≥ 660 | ≥22 | |||||
Nota: E6011 no tiene requisitos especiales para el horno de preservación de calor y Drvina: Temperatura ambiental: 20 ~ 40 C; El requisito de E6013 El horno de preservación de calor es más alto que la temperatura del marmiente [10c ~ 20c]; el secado requiere secado al menos 1 hora a 120 C150 c; E7016/E7018/E7018M Requisitos para el horno de preservación de calor y se seca; Memperatura ambiental: [30c ~ 140c]; el secado requiere secar al menos 1 ~ 2 horas a 260 ℃ ~ 425 ℃; |
mm : 0.8 mm / 0.9 mm / 1.0 mm / 1.2 mm / 1.6 mm
pulgada : 0.030 / 0.035 / 0.040 / 0.045 / 3/16 - 3/64
mm : 1.2 mm/ 1.6 mm/ 2.0 mm/ 2.4 mm/ 3.2 mm/ 4.0 mm